TY - JOUR
T1 - Effect of stress corrosion and bone regeneration on in vivo cavity in clinical osteonecrosis treatment with high-purity magnesium screws
AU - Zhang, Leyao
AU - Zhang, Yijin
AU - Sun, Jiahao
AU - Duan, Shengyu
AU - Zhao, Zeang
AU - Wang, Panding
AU - Shen, Jirong
AU - Lei, Hongshuai
N1 - Publisher Copyright:
© 2025 The Author(s)
PY - 2025/6
Y1 - 2025/6
N2 - High-purity magnesium (HP Mg) is a biodegradable metallic material, that could be applicated in implants treating osteonecrosis of the femoral head and treating peripheral artery disease. However, the degradation behavior of Mg implants was studied previously using in-vitro or in-vivo in the subcutaneous environment of rats or rabbits. This work conducted a clinical experiment on the treatment of femoral head necrosis with Ti and degradable HP Mg implants to evaluate their efficacy in enhancing surgical outcomes. During the 12-month follow-up after surgery, treatment outcomes in patients were assessed by CT, DCE-MRI and Harris hip score (HHS). The inconsistency of HP Mg degradation and bone regeneration rate induced cavities in human bodies. The effects of stress on in vitro and in vivo corrosion of Mg during implantation were investigated using experiment tests and finite element analysis. HP Mg can improve surgical effects compared to Ti in clinical applications. However, stress accelerated the corrosion of HP Mg and increased hydrogen released volume, inducing tissue and bone cavities. Stress concentration arising from cavities in adjacent bone tissue triggered localized bone density elevation and influenced osseointegration. These findings provide valuable insights into the in vivo degradation mechanisms of HP Mg in clinical applications.
AB - High-purity magnesium (HP Mg) is a biodegradable metallic material, that could be applicated in implants treating osteonecrosis of the femoral head and treating peripheral artery disease. However, the degradation behavior of Mg implants was studied previously using in-vitro or in-vivo in the subcutaneous environment of rats or rabbits. This work conducted a clinical experiment on the treatment of femoral head necrosis with Ti and degradable HP Mg implants to evaluate their efficacy in enhancing surgical outcomes. During the 12-month follow-up after surgery, treatment outcomes in patients were assessed by CT, DCE-MRI and Harris hip score (HHS). The inconsistency of HP Mg degradation and bone regeneration rate induced cavities in human bodies. The effects of stress on in vitro and in vivo corrosion of Mg during implantation were investigated using experiment tests and finite element analysis. HP Mg can improve surgical effects compared to Ti in clinical applications. However, stress accelerated the corrosion of HP Mg and increased hydrogen released volume, inducing tissue and bone cavities. Stress concentration arising from cavities in adjacent bone tissue triggered localized bone density elevation and influenced osseointegration. These findings provide valuable insights into the in vivo degradation mechanisms of HP Mg in clinical applications.
KW - Cavity
KW - High-purity magnesium
KW - Osteonecrosis of the femoral head
KW - Phenomenological corrosion model
KW - Stress corrosion
UR - http://www.scopus.com/pages/publications/105005578802
U2 - 10.1016/j.matdes.2025.114121
DO - 10.1016/j.matdes.2025.114121
M3 - Article
AN - SCOPUS:105005578802
SN - 0264-1275
VL - 254
JO - Materials and Design
JF - Materials and Design
M1 - 114121
ER -